| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.14 - 2.17 g/cc | 2.14 - 2.17 g/cc | ASTM D792 |
| Water Absorption | 0.050 % | 0.050 % | ASTM D570 |
| Deformation | 8.9 - 10.6 % | 8.9 - 10.6 % | ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 58 - 62 | 58 - 62 | ASTM D2240 |
| Ball Indentation Hardness | >= 23.0 MPa | >= 3340 psi | ISO 2032 |
| Tensile Strength at Break | >= 21.0 MPa | >= 3050 psi | ASTM D4894 |
| Elongation at Break | >= 230 % | >= 230 % | ASTM D4894 |
| Coefficient of Friction, Dynamic | 0.060 - 0.080 | 0.060 - 0.080 | ASTM D1894 |
| Coefficient of Friction, Static | 0.080 - 0.10 | 0.080 - 0.10 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
| Minimum Service Temperature, Air | -120 °C | -184 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10000 ohm-cm | 10000 ohm-cm | ASTM D257 |