| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accutech Polypropylene Homopolymer HP0334G10CL Glass Reinforced Coupled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | MD; ASTM D955 |
| Melt Flow | 5.0 g/10 min | 5.0 g/10 min | ASTM D1238 |
| Ash | 10 % | 10 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 95 | 95 | ASTM D785 |
| Tensile Strength at Break | 30.0 MPa | 4350 psi | ASTM D638 |
| Tensile Strength, Yield | 38.0 MPa | 5510 psi | ASTM D638 |
| Elongation at Break | 10 % | 10 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
| Flexural Strength | 52.0 MPa | 7540 psi | ASTM D790 |
| Flexural Modulus | 2.40 GPa | 348 ksi | ASTM D790 |
| Izod Impact, Notched | 0.342 J/cm | 0.640 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 152 °C | 306 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F |