| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech Polypropylene Homopolymer HP0334C40L1 Calcium Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.21 g/cc | 0.0437 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | MD; ASTM D955 |
| Melt Flow | 6.0 g/10 min | 6.0 g/10 min | ASTM D1238 |
| Ash | 40 % | 40 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 77 | 77 | ASTM D785 |
| Tensile Strength at Break | 15.0 MPa | 2180 psi | ASTM D638 |
| Tensile Strength, Yield | 26.0 MPa | 3770 psi | ASTM D638 |
| Elongation at Break | 40 % | 40 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 2.20 GPa | 319 ksi | ASTM D638 |
| Flexural Strength | 36.0 MPa | 5220 psi | ASTM D790 |
| Flexural Modulus | 2.499 GPa | 362.5 ksi | ASTM D790 |
| Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F |