| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech Polypropylene Copolymer CP0437G40CL Glass Reinforced Coupled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
| Ash | 40 % | 40 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 82 | 82 | ASTM D785 |
| Tensile Strength at Break | 55.0 MPa | 7980 psi | ASTM D638 |
| Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638 |
| Elongation at Break | 8.0 % | 8.0 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 4.000 GPa | 580.1 ksi | ASTM D638 |
| Flexural Strength | 80.0 MPa | 11600 psi | ASTM D790 |
| Flexural Modulus | 5.499 GPa | 797.6 ksi | ASTM D790 |
| Izod Impact, Notched | 1.92 J/cm | 3.60 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F |