| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech ABS ABS832G20L Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 0.50 g/10 min | 0.50 g/10 min | ASTM D1238 |
| Ash | 20 % | 20 % | ASTM D2584 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 102 | 102 | ASTM D785 |
| Tensile Strength at Break | 77.98 MPa | 11310 psi | ASTM D638 |
| Tensile Strength, Yield | 77.98 MPa | 11310 psi | ASTM D638 |
| Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 3.900 GPa | 565.6 ksi | ASTM D638 |
| Flexural Strength | 114.0 MPa | 16530 psi | ASTM D790 |
| Flexural Modulus | 5.699 GPa | 826.6 ksi | ASTM D790 |
| Izod Impact, Notched | 0.854 J/cm | 1.60 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 98.9 °C | 210 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 92.8 °C | 199 °F |