Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled |
Manufacturer | Aclo Compounders |
Trade Name | Accutech |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Aclo Accutech ABS ABS831G10L Glass Reinforced.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | MD; ASTM D955 |
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 105 | 105 | ASTM D785 |
Tensile Strength at Break | 56.0 MPa | 8120 psi | ASTM D638 |
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638 |
Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
Elongation at Yield | 3.0 % | 3.0 % | ASTM D638 |
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Flexural Strength | 75.01 MPa | 10880 psi | ASTM D790 |
Flexural Modulus | 3.699 GPa | 536.5 ksi | ASTM D790 |
Izod Impact, Notched | 0.908 J/cm | 1.70 ft-lb/in | ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 93.9 °C | 201 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C | 183 °F |