ATI Allvac® Grade 15-3-3-3 UNS R58153 Titanium Alloy

Category Metal , Nonferrous Metal , Titanium Alloy , Beta Titanium Alloy
Manufacturer ATI Allvac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Grade 15-3-3-3 UNS R58153 Titanium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Metastable beta titanium alloy. Uses: Industrial and aerospace components, pressure vessels, fittings, tubing, fasteners.Property values are for samples in the metallurgical condition: 1600°F anneal + water quench + age.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 4.76 g/cc
0.172 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 32
32
Tensile Strength, Ultimate 1001 MPa
145200 psi
Tensile Strength, Yield 966 MPa

@Strain 0.200 %
140000 psi

@Strain 0.200 %
Elongation at Break 8.0 %
8.0 %
Reduction of Area 10 %
10 %
Component Elements Properties Metric English Comments
Aluminum, Al 3.0 %
3.0 %
Carbon, C 0.020 %
0.020 %
Chromium, Cr 3.0 %
3.0 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe 0.12 %
0.12 %
Oxygen, O <= 0.13 %
<= 0.13 %
Tin, Sn 3.0 %
3.0 %
Titanium, Ti 76 %
76 %
as balance
Vanadium, V 15 %
15 %