Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr

Category Metal , Ferrous Metal , Stainless Steel , T S40000 Series Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low carbon, nickel containing, dual phase 12% Cr stainless steel alloy. Characteristics: superior toughness to ferritic alloys, high strength, high corrosion resistance.Information provided by Allegheny Ludlum
Mechanical Properties Metric English Comments
Hardness, Rockwell B 87
87
Tensile Strength, Ultimate 565 MPa
81900 psi
Tensile Strength, Yield 414 MPa

@Strain 0.200 %
60000 psi

@Strain 0.200 %
Elongation at Break 24 %
24 %
in 2"
Charpy Impact 67.8 J

@Temperature -73.3 °C
50.0 ft-lb

@Temperature -100 °F
Transverse
115 J

@Temperature -73.3 °C
85.0 ft-lb

@Temperature -100 °F
Longitudinal
380 J

@Temperature 15.6 °C
280 ft-lb

@Temperature 60.0 °F
Longitudinal
380 J

@Temperature 15.6 °C
280 ft-lb

@Temperature 60.0 °F
Transverse
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 11.75 %
11.75 %
Iron, Fe >= 86.13 %
>= 86.13 %
As Remainder
Manganese, Mn 0.90 %
0.90 %
Nickel, Ni 0.40 %
0.40 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si 0.70 %
0.70 %
Sulfur, S <= 0.030 %
<= 0.030 %
Users viewing this material also viewed the following: