Material Notes:
Peroxide cured, Ethylene Propylene Terpolymer, 46-55 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Complies with FDA code of Federal regulations title CFR21 section 177.2600. Water and n-hexane tested. Also complies to the requirements of USP 25, NF20, 2002, Class 6. To meet ASTM D2000/SAE J200 line call-out M3CA507, A25, B35, EA14, F17.Applications: Excellent water and steam resistance with good compression set properties. Heat and chemical resistance is superior to that of sulphur cured EPDM. Not oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 53
53
°IRHD; ASTM D1415
58
58
°IRHD, +5 change after 70 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D412
11.5 MPa
1670 psi
15% change after 70 hours @ 125°C; ASTM D412
Elongation at Break 340 %
340 %
-15% change after 70 hours @ 125°C; ASTM D412
400 %
400 %
ASTM D412
Compression Set 30 %
30 %
22 hours @ 125°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F
Descriptive Properties Value Comments
Extraction Test, 21 CFR 177.2600 pass
Distilled Water
pass