0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.." />
Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel ASTM A 570, Grade 33 Hot Rolled Carbon Steel, Structural Quality (SQ)

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ASTM A 570, Grade 33 Hot Rolled Carbon Steel, Structural Quality (SQ).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 360 MPa
>= 52200 psi
Tensile Strength, Yield >= 230 MPa
>= 33400 psi
Elongation at Break >= 23 %
>= 23 %
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000142 ohm-cm
0.0000142 ohm-cm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved