| Category | Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel |
| Manufacturer | AK Steel |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | AK Steel ASTM A 1011, Grade 33 Hot Rolled Carbon Steel, Structural Steel (SS).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.87 g/cc <br>@Temperature 20.0 °C |
0.284 lb/in³ <br>@Temperature 68.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | >= 360 MPa | >= 52200 psi | |
| Tensile Strength, Yield | >= 230 MPa | >= 33400 psi | |
| Elongation at Break | >= 23 % | >= 23 % | |
| Modulus of Elasticity | 200 GPa <br>@Temperature 20.0 °C |
29000 ksi <br>@Temperature 68.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 12.4 µm/m-°C <br>@Temperature 20.0 - 100 °C |
6.89 µin/in-°F <br>@Temperature 68.0 - 212 °F |
|
| Specific Heat Capacity | 0.481 J/g-°C <br>@Temperature 50.0 - 100 °C |
0.115 BTU/lb-°F <br>@Temperature 122 - 212 °F |
|
| Thermal Conductivity | 89.0 W/m-K <br>@Temperature 20.0 °C |
618 BTU-in/hr-ft²-°F <br>@Temperature 68.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.000142 ohm-cm <br>@Temperature 20.0 °C |
0.000142 ohm-cm <br>@Temperature 68.0 °F |