S&E Specialty Polymers TufTech™ G-3489 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ G-3489 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: A general purpose PVC based flexible compound designed for profile extrusion.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89.0

@Time 15.0 sec
89.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 17.6 MPa
2550 psi
ASTM D412
Elongation at Break 325 %
325 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 174 - 179 °C
345 - 355 °F
Suggested Stock