Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness

Category Polymer , Thermoset , Polyimide, TS , Polyimide, Thermoset Film
Manufacturer CEN® Electronic Material Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With superior dimensional stability at elevated temperatures, CEN®CV polyimide film is ideal for high temperature applications that require a low-shrinkage film.Applications: sensors, gaskets, electronic parts, pin grids, coverlay film, TAB tapes, reinforced board for FPCAll information provided by CEN Electronic Material Co., LTD.
Physical Properties Metric English Comments
Thickness 46.0 - 54.0 microns
1.81 - 2.13 mil
ASTM D374
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 160 MPa
23200 psi
ASTM D882
Film Tensile Strength at Yield, TD 150 MPa
21800 psi
ASTM D882
Film Elongation at Yield, MD >= 50 %
>= 50 %
ASTM D882
Film Elongation at Yield, TD >= 55 %
>= 55 %
ASTM D882
Electrical Properties Metric English Comments
Volume Resistivity >= 8.00e+13 ohm-cm
>= 8.00e+13 ohm-cm
ASTM D257
Surface Resistance >= 8.00e+14 ohm
>= 8.00e+14 ohm
ASTM D257
Dielectric Strength >= 180 kV/mm
>= 4570 kV/in
ASTM D149