Data provided by the manufacturer, ComAlloy International Company.25% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 107 MPa
15500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 169 MPa
24500 psi
ASTM D790
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.37 J/cm
13.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 258 - 268 °C
496 - 514 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 191 °C
376 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F