Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchlite™ S60/10000 Glass Bubbles

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer 3M
Trade Name Scotchlite™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchlite™ S60/10000 Glass Bubbles.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High-strength polymer additives made from a water-resistant and chemically-stable soda-lime-borosilicate glass. These hollow glass microspheres can be used as a low density filler material ideal for plastic and rubber parts created from injection molding, extrusion processes and/or other vigorous processing equipment (Banbury mixers, etc.). Scotchlite glass bubbles help to reduce weight; reduce thermal expansion; and contribute to cost savings. They are used as additive materials in the automotive, truck, rail and aerospace industries.Information supplied by 3M Specialty Materials.
Physical Properties Metric English Comments
Density 0.600 g/cc
0.0217 lb/in³
True Density
Bulk Factor 0.63
0.63
Packing factor (bulk density to true particle density)
Oil Absorption 33.5 %
33.5 %
g oil/100 cc of polymer additive
Loss On Ignition <= 0.50 %
<= 0.50 %
Volatile content (by weight)
Particle Size 30 µm
30 µm
Average diameter
pH 9.5
9.5
at 5% loading in water
Mechanical Properties Metric English Comments
Compressive Strength 68.9 MPa
10000 psi
Isostatic crush strength
Thermal Properties Metric English Comments
Softening Point 600 °C
1110 °F
Descriptive Properties Value Comments
Alkalinity 0.5 milliequivalents/gram max.
Color, Unaided Eye White, powdery
Composition Soda-lime-borosilicate glass
Flotation (density 92% (in volume)
Shape Hollow glass spheres with thin walls
Users viewing this material also viewed the following: