Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchlite™ IJ5100-10 Reflective Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name Scotchlite™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchlite™ IJ5100-10 Reflective Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects white); Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Version for screen printing and thermal mass transfer, inkjet printing, and electrostatic imaging; Designed for excellent cutting and weeding with computer sign cutting equipment; For vertical, flat or curved surfaces with or without rivets; Unprocessed film resists fuel vapors or occasional spills.Information provided by 3M
Mechanical Properties Metric English Comments
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to FRP
0.789 kN/m
4.50 pli
Adhesion to Painted aluminum panels
1.05 kN/m
6.00 pli
Adhesion to Aluminum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 29.0 °C
84.2 °F
Air and substrates, for flat surfaces without rivets
29.0 °C
84.2 °F
Air and substrates, for flat surfaces with rivets
38.0 °C
100 °F
Dry; flat, curved or corrugated surfaces with rivets
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Air and substrates, for flat surfaces without rivets
13.0 °C
55.4 °F
Dry; flat, curved or corrugated surfaces with rivets
13.0 °C
55.4 °F
Air and substrates, for flat surfaces with rivets