3M Scotchkote™ PR 504 Urethane Pipe Repair

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ PR 504 Urethane Pipe Repair.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Urethane Pipe Repair PR 504 is a special fast curing moisture activated repair bandage for repair bandage for repairs to leaking pipes.Product Features:Easy to apply, requiring no special tools or equipment. Specially selected woven polyester fabric impregnated with a polyurethane resin which is activated by immersion in water.Ideal for repairing pipes operating at low pressuresDesigned for use for repairs to pipes up to 65 mm diameterCan be used on a wide variety of surfaces, including all metals and many types of plastic Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Flexural Strength 32.0 MPa
4640 psi
Compressive Strength 19.00 MPa
2755 psi
Processing Properties Metric English Comments
Cure Time 5.0000 min
0.083333 hour
Initial Set
30.0 min
0.500 hour
Full Mechanical
Descriptive Properties Value Comments
Appearance Off white