Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible XV3919 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne Geon™ Vinyl Flexible XV3919 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
15 sec; ASTM D2240
93
93
ASTM D2240
Hardness, Shore D 33
33
15 sec; ASTM D2240
48
48
ASTM D2240
Tensile Strength at Break 19.0 MPa

@Temperature 23.0 °C
2760 psi

@Temperature 73.4 °F
510 mm/min; ASTM D638
Elongation at Break 310 %

@Temperature 23.0 °C
310 %

@Temperature 73.4 °F
510 mm/min; ASTM D638
Tensile Modulus 0.0121 GPa

@Temperature 23.0 °C
1.75 ksi

@Temperature 73.4 °F
510 mm/min100% Secant; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -19.4 °C
-2.92 °F
ASTM D746
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Features Good Chemical Resistance
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following: