3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Ceramic HD Surfacer HG 519 has been specifically developed as a 100% solids ceramic repair system for resurfacing equipment subject to severe abrasion.Product Features:Combines good application characteristics with excellent build capabilities.Designed for application by trowel or spatula at thicknesses up to 12 mmProvides outstanding resistance to sliding abrasionDesigned for use to rebuild worn hoppers, chutes, pipe elbows and other equipment subject to aggressive attack from dry solids and slurriesExcellent adhesion to correctly prepared metal surfaces Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness <= 152 microns
<= 6.00 mil
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Flexural Strength 41.4 MPa
6000 psi
ASTM D790
Compressive Strength 103 MPa
15000 psi
ASTM D695
Shear Strength 13.8 MPa
2000 psi
Tensile Shear Adhesion, on a grit blasted steel; ASTM D1002
Abrasion 1.1
1.1
[g] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 158 °C
316 °F
Wet
248 °C
478 °F
Dry
Heat Distortion Temperature 60.0 °C
140 °F
ASTM D648
Processing Properties Metric English Comments
Cure Time 480 min
8.00 hour
Hard Dry for machining
7200 min
120 hour
Full Cure
Descriptive Properties Value Comments
Appearance Gray