3M Scotch-Weld™ AC113 Instant Adhesive Primer

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ AC113 Instant Adhesive Primer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Scotch-Weld™ Instant Adhesive Activator AC113 is heptane based. Generally this activator will not attack plasticsInformation provided by 3M
Physical Properties Metric English Comments
Density 0.680 g/cc
0.0246 lb/in³
Viscosity <= 1.0 cP
<= 1.0 cP
Descriptive Properties Value Comments
Appearance Colorless to Pale Yellow Liquid