3M RJS-2 3/C Phase Rejacketing System

Category Other Engineering Material
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M RJS-2 3/C Phase Rejacketing System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M RJS Series Rejacking Sleeves are dinged so that 3M Cold Shrink QTII and QTIII Silicone Rubber Termination applications can be used on 3/C (three conductor) medium voltage shielded power cables of tape shield, wire shield, armored and non-armored confiations. RJS Rejacketing Assemblies are a series of silicone rubber insulator incorporating an inner expandable polyester braid designed to reduce sliding friction and deliver the insulator onto the cable. Rejacketing sleeves are designed to protect the phase legs (core) of 3/C shielded power cable from exposure to moisture, corrosion, ozone, ultra-violet radiation, physical contact and other hazards that are associated with termination operating environments. Rejacketing sleeves are designed to be used in conjunction with 3M Cold Shrink Breakout Boots and Silicone Rubber Terminations.Information provided by 3M
Physical Properties Metric English Comments
Thickness 16.5 microns
0.650 mil
Wall
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.295 MPa
1058 psi
ASTM D412
Elongation at Break 910 %
910 %
ASTM D412
50% Modulus 0.000220 GPa
0.0319 ksi
ASTM D412
100% Modulus 0.000310 GPa
0.0450 ksi
ASTM D412
Tear Strength 31.4 kN/m
179 pli
ASTM D624 B
Electrical Properties Metric English Comments
Dielectric Strength 16.9 kV/mm

@Thickness 1.65 mm
428 kV/in

@Thickness 0.0650 in
Track Resistance 21600 sec
21600 sec
ASTM D2303/IEC 587
Descriptive Properties Value Comments
Appearance Dark Gray