| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | 3M |
| Trade Name | Nextel™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | 3M Nextel™ XN-625 Woven Fabric 720.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.40 g/cc | 0.123 lb/in³ | |
| Permeability | 30 | 30 | [ft<sup>3</sup>/min/ft<sup>2</sup>], Air w/o sizing |
| Thickness | 560 microns | 22.0 mil | |
| Fiber Count | 3330 dtex | 3000 denier | roving |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 2100 MPa | 305000 psi | filament 25.4mm |
| Tensile Modulus | 248 GPa | 36000 ksi | filament |
| Tear Strength | 31.4 kN/m | 179 pli | Warp, Breaking Strength w/o Sizing |
| 31.4 kN/m | 179 pli | Fill, Breaking Strength w/o Sizing |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.00 µm/m-°C @Temperature 100 - 1100 °C |
3.33 µin/in-°F @Temperature 212 - 2010 °F |
|
| Melting Point | 1800 °C | 3270 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.67 | 1.67 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 85 % | 85 % | |
| SiO2 | 15 % | 15 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 5.8 @Frequency 9.375e+9 Hz |
5.8 @Frequency 9.375e+9 Hz |