Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ TF 2053Z PTFE Fine Powder

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 2053Z PTFE Fine Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dyneon™ TF 2053 Z PTFE is an ideal grade for extrusion of tubing and cables requiring only moderately high reduction ratio.Product Features:Processable by standard paste extrusion methods Good overall balance of mechanical properties and processabilityEmulsion Polymerization PTFEMeets ASTM D4895-04 Type 1, Grade 1, C Class C classificationInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
ISO 12086
Density 2.16 g/cc
0.0780 lb/in³
DIN EN ISO 12086
Particle Size 520 µm
520 µm
average; ISO 13320
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.0 MPa
4640 psi
DIN EN ISO 527-3
Elongation at Break 390 %
390 %
DIN EN ISO 527-3
Descriptive Properties Value Comments
Extrusion Pressure, 65 MPa
ASTM D4895
Reduction Ratio Range 20-1200:1
(Dyneon Method)