Material Notes:
3M™ Dyneon™ PVDF 2066/0002, a fluoropolymer material, provides an excellent balance of physical properties, processability, surface smoothness, flexibility, and refractive index, allowing for a wide array of gauges for filaments such as fishing line. In addition to the well established intrinsic characteristics of PVDF such as high strength for a given filament diameter and a refractive index nearly identical to water, PVDF 2066/0002 has improved impact resistance that can provide additional shock strength to filamentFeatures and Benefits:Highest impact strength of any extrudable 3M PVDFHighest melt viscosity of any extrudable 3M PVDFHigh tensile strengthInformation provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Melt Flow 4.0 - 6.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
4.0 - 6.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.0 MPa
9720 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 46.0 MPa
6670 psi
50 mm/min; ASTM D638
Elongation at Break 428 %
428 %
50 mm/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.67 GPa
242 ksi
50 mm/min; ASTM D790
Descriptive Properties Value Comments
Color Opaque
Volatile Matter <0.2%
5 min/110°, Thermobalance