Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 3381 HVAC Construction

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 3381 HVAC Construction.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Value grade aluminum foil tape. UL 723 ClassifiedInformation provided by 3M
Physical Properties Metric English Comments
Thickness 35.6 microns
1.40 mil
Backing; ASTM D3652
76.2 microns
3.00 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.7 MPa
3440 psi
ASTM D3759
Peel Strength 0.438 kN/m
2.50 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Adhesive Type Acrylic
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved