3A Composites Core Materials BALTEK® SB.150 Structural End-Grain Balsa

Category Other Engineering Material , Composite Core Material , Wood and Natural Products , Wood , Hardwood
Manufacturer 3A Composites Core Materials
Trade Name BALTEK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3A Composites Core Materials BALTEK® SB.150 Structural End-Grain Balsa.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent bond with all types of resins and adhesives. It is compatible with a variety of manufacturing processes and is resistant to temperature changes, or exposure to fire, or chemicals such as styrene. BALTEK SB is an ideal core material for an extensive range of applications. All while being a renewable resource.Characteristics: Extremely high strength and stiffness to weight ratiosExcellent fire performanceEcological productWide operating temperature range -212 °C to +163 ° C (-414 °F to +325 °F)Excellent fatigue resistanceGood sound and thermal insulationHigh impact strengthGood moisture resistanceApplicationsMarine: Hulls, decks, bulkheads, superstructures, interiors, tooling + moldsRoad and Rail: Floors, walls, roof panels, body panels, interiors, front-ends, side skirtsWind Energy: Rotor blades, spinners, nacelle covers, generator housingsAircraft: Floor panels, galley carts, interior partitions, cargo pallets, containers, general aviation (sport aircraft) partsDefense: Naval vessels, containers, cargo pallets, sheltersIndustrial: Tooling, tanks, ductwork, impact limiter, concrete forms, fascia panels, skis, snowboards, wakeboards
Physical Properties Metric English Comments
Density 0.247 g/cc
0.00892 lb/in³
apparent nominal; ASTM C271
Mechanical Properties Metric English Comments
Tensile Strength 23.5 MPa
3410 psi
perpendicular to plane; ASTM C297
Tensile Modulus 5.759 GPa
835.3 ksi
perpendicular to plane; ASTM C297
Compressive Strength 26.3 MPa
3810 psi
perpendicular to plane; ASTM C365
Compressive Modulus 7.982 GPa
1158 ksi
perpendicular to plane; ASTM C365
Shear Modulus 0.309 GPa
44.8 ksi
ASTM C273
Shear Strength 4.90 MPa
711 psi
ASTM C273
Thermal Properties Metric English Comments
Thermal Conductivity 0.0840 W/m-K
0.583 BTU-in/hr-ft²-°F
ASTM C177