BASF
BASF > Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Manufacturer :
BASF
>
Category :
Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Product List
Tips:
Up to 100 items are displayed.
PRODUCT NO.
Category
Trade Name
BASF Luranyl® KR 2403 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced
Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Luranyl®
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced
Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Luranyl®
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Luranyl®
BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced
Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Luranyl®
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
Luranyl®