Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 130 °C |
5.00e+13 ohm-cm @Temperature 266 °F |
ASTM D257 |
Lord Adhesives Thermoset™ UR-322 Two Component Urethane Potting Compound Lord UR-322 is a two component, room temperature curing urethane potting compound. The cured elastomer is soft, flexible and has a very low modulus at temperatures down to -80°C. Cured UR-322 als.. |
|||
Volume Resistivity | >= 5.00e+13 ohm-cm @Temperature 20.0 °C |
>= 5.00e+13 ohm-cm @Temperature 68.0 °F |
|
Sibur 140-13A Compound 8/2 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | >= 5.00e+13 ohm-cm @Temperature 20.0 °C |
>= 5.00e+13 ohm-cm @Temperature 68.0 °F |
|
Sibur 140-13P Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 20.0 °C |
5.00e+13 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 60.0 °C |
5.00e+13 ohm-cm @Temperature 140 °F |
JIS-K-6723 |
Denka VINYKON W1051 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 60.0 °C |
5.00e+13 ohm-cm @Temperature 140 °F |
JIS-K-6723 |
Denka VINYKON W4050 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |