Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 - 5.00e+12 ohm-cm | 1.00e+11 - 5.00e+12 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTU PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency, UV cut, and superior cleanliness for advanced semiconductor packaging applications |
|||
Volume Resistivity | 3.00e+12 - 5.00e+12 ohm-cm | 3.00e+12 - 5.00e+12 ohm-cm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Volume Resistivity | 3.00e+12 - 5.00e+12 ohm-cm | 3.00e+12 - 5.00e+12 ohm-cm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Volume Resistivity | 3.00e+12 - 5.00e+12 ohm-cm | 3.00e+12 - 5.00e+12 ohm-cm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Volume Resistivity | 3.00e+12 - 5.00e+12 ohm-cm | 3.00e+12 - 5.00e+12 ohm-cm | DIN 53482 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |