Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group AMPLA® 2500 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
PolyOne Edgetek® NL-08GF-02CF/000 Nylon 6/12, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0177 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0254 C 75% Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium Sulfate, 75% Filler by WeightFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0266 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0177 B Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0249 B Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PET 0268 B1 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® POM 0223 B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0180 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0201 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0254 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+13 - 1.00e+14 ohm-cm | 1.00e+13 - 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |