Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 20GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm @Temperature 25.0 °C |
2.50e+15 ohm-cm @Temperature 77.0 °F |
ASTM D257 |
Lord Adhesives Thermosetâ„¢ SC-102 Unfilled Silicone Encapsulant Lord SC-102 is a "water-white" clear, two component, silicone encapsulating system. It has a very low viscosity and, when cured, a low Shore A hardness. Lord SC-102 is optically transparent with no .. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | |
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM UF5011S PEI Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCD851 PPE-TPE (Asia Pacific) Flexible, strong flame-retardant, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | |
Tra-Con Tra-Bond 2248 High Temperature Epoxy Staking Adhesive TRA-BOND 2248 is a thixotropic, high temperature cure, 100% solids epoxy resin system that provides strong, tough bonds between a wide range of materials (includes metals, glass, ceramics, and many .. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | |
Tra-Con Tra-Bond F211 General Purpose Fiber Optic Epoxy Adhesive TRA-BOND F211 is a general purpose fiber optic epoxy adhesive recommended for bonding and small volume potting applications where superior wetting and physical properties are needed at both high and.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | |
Tra-Con Tra-Bond 2211 High Temperature Epoxy Adhesive TRA-BOND 2211 is a low viscosity epoxy adhesive system recommended for industrial bonding applications where superior wetting and good mechanical and electrical insulation performance features are r.. |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | |
Dow Corning Q2-7735 ADHESIVE Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning |
|||
Volume Resistivity | 2.50e+15 ohm-cm | 2.50e+15 ohm-cm | Cond. C (96 hrs/23°C/96% rel. humidity) |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |