Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1e+15 - 1e+16 ohm-cm | 1e+15 - 1e+16 ohm-cm | ASTM D257 |
Kureha KF Polymer 1100 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Volume Resistivity | 1e+15 - 1e+16 ohm-cm | 1e+15 - 1e+16 ohm-cm | ASTM D257 |
Kureha KF Polymer 850 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Volume Resistivity | 1e+15 - 1e+16 ohm-cm | 1e+15 - 1e+16 ohm-cm | ASTM D257 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Volume Resistivity | 1e+15 - 1e+16 ohm-cm | 1e+15 - 1e+16 ohm-cm | ASTM D257 |
Kureha KF Polymer 1300 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Volume Resistivity | 1e+15 - 1e+16 ohm-cm | 1e+15 - 1e+16 ohm-cm | ASTM D257 |
Kureha KF Polymer 2950 PVDF Copolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Volume Resistivity | >= 1e+15 ohm-cm @Temperature 25.0 °C |
>= 1e+15 ohm-cm @Temperature 77.0 °F |
|
Master Bond MB250NT Low viscosity ethyl cyanoacrylate Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi.. |
|||
Volume Resistivity | >= 1e+15 ohm-cm | >= 1e+15 ohm-cm | |
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system Cures at room temperature to form a soft, resilient gel-like system with good dimensional stability. It has excellent optical clarity, convenient to handle, and is easy to retrieve with a sharp kni.. |