Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Cond. A; IPC 2.5.17.1 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm | >= 1.00e+9 ohm-cm | ASTM D257-91 |
NeXolve LaRC™-CP1 Polyimide Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF33 NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightUL File Number: E157318Appearance: Black and Natural ColorTPCI# 9475101Information provi.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF60 HS UV BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Volume Resistivity | >= 1.00e+9 ohm-cm | >= 1.00e+9 ohm-cm | |
Sibur Phenoplast For production by direct pressing. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+10 ohm-cm | 1.00e+9 - 1.00e+10 ohm-cm | ASTM D257 |
Supreme Petrochem SP 6520 Permanent Antistatic Polystyrene Characteristics No sloughing Fully colorable Meets MIL-PRF-81705D static decay specification Functions even in low humidity levels Processing Injection molding Extrusion & Forming Applications C.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static) Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Practical Use (Water Absorption 2.3%); ASTM-D257 |
Toyobo GLAMIDE® T-422-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+10 ohm-cm | 1.00e+9 - 1.00e+10 ohm-cm | Practical Use (Water Absorption 2.5%); ASTM-D257 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+10 ohm-cm | 1.00e+9 - 1.00e+10 ohm-cm | Practical Use (Water Absorption 2.1%); ASTM-D257 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Practical Use (Water Absorption 1.6%); ASTM-D257 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Practical Use (Water Absorption 2.0%); ASTM-D257 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Cotronics Resbond™ 907 High Temperature Ceramic Adhesive, Industrial Strength |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | cond; IEC 60093 |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned) Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate High Density, high strength molding compound. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | Practical Use (Water Absorption 2.8%); ASTM-D257 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | IEC 60093 |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |