Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir N 1782 Polystyrene General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir N 1840 Polystyrene General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir R 321P Polystyrene Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RK 451G Polystyrene UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded, high impact polystyrene. This grade combines medium flow, heat resistance and good light stability for injection moulding of technical p.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RT 441M Polystyrene High impact polystyrene combining high toughness and high stiffness with good flowability for easy processing. Designed for injection moulding of technical parts, housings and covers.
Especially rec.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RT 461F Polystyrene High impact, heat resistant polystyrene with good stiffness. Recommended for improving the thermal performance of injection moulded technical parts which are submitted to high temperature in service.. |
|||
Volume Resistivity | >= 7.00e+15 ohm-cm | >= 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR Very high environmental stress cracking resistant (VH ESCR) HIPS.ICE S 900 exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents, and in particular to cyclopent.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir N 2380 Polystyrene High molecular weight general purpose polystyrene combining high heat resistance and good mechanical strength. Suitable for direct gassing extrusion, for biaxially oriented films and sheets, for gla.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir RKL Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Volume Resistivity | >= 7.00e+15 ohm-cm | >= 7.00e+15 ohm-cm | ASTM D257 |
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PC/PBT IM 1012 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PC/PET IM 1016 UV Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ PE450B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | |
Dow Corning SE 4445 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility, UL V-0.Information provided by Dow Corning |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1001 XV is a C4 Ziegler Natta LLDPE for power cable and Telecom jacketing. The grade contains a low level of antioxidants and has excellent Environmental Stress Crack Resista.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 6101RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 6101XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | ASTM D257 |
ExxonMobil LLDPE LL 6301XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | |
Dow Corning 3-4150 DIELECTRIC GEL KIT Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning |
|||
Volume Resistivity | 7.00e+15 ohm-cm | 7.00e+15 ohm-cm | IEC 60093 |
Polimeri Europa Edistir N 1910 Polystyrene Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear.. |