Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.90e+13 ohm-cm | 5.90e+13 ohm-cm | ASTM D257 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Volume Resistivity | 5.90e+13 ohm-cm | 5.90e+13 ohm-cm | |
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system .. |
|||
Volume Resistivity | 5.90e+13 ohm-cm | 5.90e+13 ohm-cm | ASTM D257 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |