Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | STN IEC 60093 |
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | |
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | STN IEC 60093 |
Plastcom SLOVAMID 6 GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | 70°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Volume Resistivity | >= 5.00e+13 ohm-cm | >= 5.00e+13 ohm-cm | NBR 5403 |
Karina E 75800-35/1-B-AC Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® ASA FR-2 WT Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® ASA FR-2A WT209 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant, Good Toughness and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill® ASA 778 UV WT168 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill® ASA 814 GY Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | >= 5.00e+13 ohm-cm | >= 5.00e+13 ohm-cm | |
Sibur PVC S-7059-M Suspension Polyvinyl Chloride (PVC) For production of articles by methods of extrusion, calendaring, pressing, rolling, or molding under pressure. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | IEC 93 |
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac RX 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | IEC 60093 |
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 20.0 °C |
5.00e+13 ohm-cm @Temperature 68.0 °F |
BS 2782 |
Teknor Apex Sinvicomp SIM 5029 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 20.0 °C |
5.00e+13 ohm-cm @Temperature 68.0 °F |
BS 2782 |
Teknor Apex Sinvicomp SIM 5039 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 20.0 °C |
5.00e+13 ohm-cm @Temperature 68.0 °F |
BS 2782 |
Teknor Apex Sinvicomp SIM 5515 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | |
Master Bond Mastersil 150 Two Part, Condensation Cured, Flexible Silicone Master Sil 150 is a 2 part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | ASTM D247 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | IEC 60093 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | IEC 60093 |
Polyplastics Duracon® TD-30 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 30.0 °C |
5.00e+13 ohm-cm @Temperature 86.0 °F |
JIS-K-6723 |
Denka VINYKON W3012 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 23.0 °C |
5.00e+13 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FK 86 Flexible PVC, Insulation Lead Free General purposes |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 23.0 °C |
5.00e+13 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FR 008 Flexible PVC, Insulation Insulation |
|||
Volume Resistivity | >= 5.00e+13 ohm-cm | >= 5.00e+13 ohm-cm | |
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm | 5.00e+13 ohm-cm | 50% RH; ASTM D-257 |
Axiall 11800 Wire & Cable Flexible PVC Designed for 75°C rated cords and cord sets and other general purpose insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Volume Resistivity | >= 5.00e+13 ohm-cm | >= 5.00e+13 ohm-cm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Volume Resistivity | 5.00e+13 ohm-cm @Temperature 23.0 °C |
5.00e+13 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 93 Flexible PVC, Flame Retardant Insulation General purposes |