Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.70e+15 ohm-cm | 4.70e+15 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Volume Resistivity | 4.70e+15 ohm-cm | 4.70e+15 ohm-cm | |
Dow Corning 3-4133 DIELECTRIC GEL KIT Two-part, clear, heat cure, and firm.Information provided by Dow Corning |
|||
Volume Resistivity | 4.70e+15 ohm-cm | 4.70e+15 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
Volume Resistivity | 4.70e+15 ohm-cm | 4.70e+15 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |