Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.10e+14 ohm-cm | 4.10e+14 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Volume Resistivity | 4.10e+14 ohm-cm | 4.10e+14 ohm-cm | ASTM D257 |
3M Scotch-Weld™ DP270 Clear Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Volume Resistivity | 4.10e+14 ohm-cm | 4.10e+14 ohm-cm | |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |
|||
Volume Resistivity | 4.10e+14 ohm-cm | 4.10e+14 ohm-cm | |
Resinlab® EP1300 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Clear (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |