Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.4 kV/mm @Thickness 3.20 mm |
493 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Dielectric Strength | 19.4 kV/mm @Thickness 3.20 mm |
493 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Dielectric Strength | 19.4 kV/mm @Thickness 3.20 mm |
493 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Dielectric Strength | 19.4 kV/mm @Thickness 3.20 mm |
493 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Dielectric Strength | 19.4 kV/mm | 493 kV/in | Short Time; ASTM D149 |
Plenco 50335 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |