Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.4 kV/mm | 365 kV/in | |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Dielectric Strength | 14.4 - 51.2 kV/mm | 365 - 1300 kV/in | Average value: 23.2 kV/mm Grade Count:38 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | |
Dow Corning SE 4422 SILICONE RTV One-part, grey, moisture cure RTV, flowable, thermally conductive, UL V-1.Information provided by Dow Corning |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | ASTM D149 |
Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production ma.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | ASTM D149 |
Arlon R36319R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QI-18/57-325 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QI-5/16-220 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M SJ-3A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 14.4 - 16.3 kV/mm | 365 - 415 kV/in | short time |
Bulk Molding Compounds BMC T14 General Purpose Molding Compound BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D-149 |
3M 5300 Motor Lead Splicing Kits 3M Motor Lead Splicing Kits 5300 Series are a series of kits designed for splicing motor lead cables to incoming feeder cables. The kits accommodate the follow splice confiations:Pigtails (stub) con.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8420-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8424-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8425-8 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8427-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8427-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8428-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8428-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8428-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-12 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8452 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8454 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QI-10/37-270 Cold Shrink Quick Insulator 3M™ Cold Shrink Quick Insulator QI Series are open-ended tubular rubber sleeves with sealing mastic on each end that are factory expanded and assembled onto a removable core. The core is removed by.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QSLV-M-2-500 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Dielectric Strength | 14.4 kV/mm | 365 kV/in | Original; ASTM D149-75 |
3M QSLV-M-8-2/0 Cold Shrink Quick Splice Low Voltage 3M™ Cold Shrink Quick Splice Low Voltage QSLV-M are open-ended tubular rubber sleeves with sealing mastic on each end which are factory expanded and assembled onto a unique three-core system. Two c.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M SJ-1A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Dielectric Strength | 14.4 - 16.3 kV/mm | 365 - 415 kV/in | short time |
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8427-16 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8429-9 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Dielectric Strength | 14.4 kV/mm @Thickness 1.78 mm |
365 kV/in @Thickness 0.0700 in |
Original; ASTM D149-75 |
3M 8461 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |