Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® CYNERGY CA6401 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® CYNERGY CA6402 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Dielectric Strength | 13.8 - 105 kV/mm | 350 - 2670 kV/in | Average value: 28.7 kV/mm Grade Count:20 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Dielectric Strength | 13.8 - 24.0 kV/mm | 350 - 610 kV/in | Average value: 16.0 kV/mm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Dielectric Strength | 13.8 - 19.7 kV/mm | 350 - 500 kV/in | Average value: 15.3 kV/mm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Rubber Repair / Castable Urethane High Temp Edge & Seal (T-36), Amber Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Term |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Cytec (Conap) RN-1200 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Dielectric Strength | 13.8 - 17.7 kV/mm @Thickness 3.17 mm |
350 - 450 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 55869R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Dielectric Strength | 13.8 - 14.6 kV/mm | 350 - 370 kV/in | Short Time |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Dielectric Strength | 13.8 - 15.0 kV/mm | 350 - 380 kV/in | Short Time |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Time |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Dielectric Strength | >= 13.8 kV/mm | >= 350 kV/in | Short Time |
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Time |
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | S/T |
Abatron AboCast 8103-30 High-Performance Dielectric Epoxy AboCast 8103-30 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Arlon R30370A015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Dielectric Strength | 13.8 - 15.0 kV/mm | 350 - 380 kV/in | Short Time |
Bulk Molding Compounds BMC 5338 Mineral Filled, Glass Reinforced Polyester BMC 5338 molding compound is a mineral Filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Dielectric Strength | 13.8 - 15.0 kV/mm | 350 - 380 kV/in | short time |
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming 2741-15 Stycast® Two-Component Epoxy Flexible EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components wh.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |