Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.00 - 14.6 kV/mm | 25.4 - 371 kV/in | Average value: 5.72 kV/mm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Strength | 1.00 - 100 kV/mm | 25.4 - 2540 kV/in | Average value: 33.0 kV/mm Grade Count:193 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Dielectric Strength | 1.00 kV/mm @Diameter >=3.00 mm |
25.4 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronit B 65 Phenolic, Paper Reinforcement, Dark Brown, Tubes Description: For mechanical and electrical low-voltage applications. Good electrical properties at normal air humidity.Applications: Winding tubes in the foil and metal foil industries and carrier t.. |
|||
Dielectric Strength | 1.00 kV/mm @Diameter >=3.00 mm |
25.4 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Tubes Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig.. |
|||
Dielectric Strength | 1.00 kV/mm @Diameter >=3.00 mm |
25.4 kV/in @Diameter >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronit IV C S Phenolic, Paper Reinforcement, Black, Tubes Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig.. |
|||
Dielectric Strength | 1.00 kV/mm | 25.4 kV/in | |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Dielectric Strength | 1.00 kV/mm | 25.4 kV/in | |