Electrical Properties Metric English Comments
Dielectric Strength 9.40 kV/mm
239 kV/in
Short Time; Dry; ASTM D149
Resinoid 1370 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Dielectric Strength 9.40 kV/mm

@Thickness 2.50 mm
239 kV/in

@Thickness 0.0984 in
DC @ 0.100 in (2.5 mm) thickness
MarkeTech Aluminum Oxide Ceramic - Alumina 98%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
Dielectric Strength 9.40 kV/mm
239 kV/in
ICE Steatite L-4
Data provided by the manufacturer, International Ceramic Engineering.
Dielectric Strength 9.40 kV/mm
239 kV/in
ICE Steatite L-5
Data provided by the manufacturer, International Ceramic Engineering.
Dielectric Strength 9.40 kV/mm
239 kV/in
Short Time; ASTM D149
Plenco 3303 Phenolic, Granular, Injection Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
Dielectric Strength 9.40 kV/mm
239 kV/in
Short Time; ASTM D149
Plenco 4527 Phenolic, Granular, Injection Molded
PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under..
Dielectric Strength 9.40 kV/mm
239 kV/in
ac; ASTM D116
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 9.40 kV/mm
239 kV/in
AC; ASTM D116
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 9.40 kV/mm
239 kV/in
ac; ASTM D116
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Dielectric Strength 9.40 kV/mm
239 kV/in
Du-Co Ceramics CS-144-L-5 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Dielectric Strength 9.40 kV/mm
239 kV/in
Short Time; Dry; ASTM D149
Resinoid 1322 Phenolic Molding, Glass Reinforced