Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 5.50 kV/mm | 140 kV/in | AC 60 Hz; 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 5.50 kV/mm | 140 kV/in | Step by Step; ASTM D149 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Dielectric Strength | 5.50 kV/mm | 140 kV/in | ASTM D149 |
Tipco Tipcolite® TMS 311 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D149 |
3M 4516 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 5.50 - 7.50 kV/mm @Temperature 90.0 °C |
140 - 191 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Dielectric Strength | 5.50 - 7.00 kV/mm @Temperature 90.0 °C |
140 - 178 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Dielectric Strength | 5.50 - 7.50 kV/mm @Temperature 90.0 °C |
140 - 191 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Dielectric Strength | 5.51 kV/mm | 140 kV/in | ASTM D1000 |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 5.50 kV/mm | 140 kV/in | ST; ASTM D149 |
Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Mil.. |