Polymer Property : Dielectric Strength = 7.90 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 7.90 - 15.0 kV/mm
201 - 381 kV/in
Average value: 12.3 kV/mm Grade Count:19
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Dielectric Strength 7.90 - 16.2 kV/mm
201 - 411 kV/in
Average value: 11.1 kV/mm Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Dielectric Strength 7.90 - 36.0 kV/mm
201 - 914 kV/in
Average value: 16.0 kV/mm Grade Count:55
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Dielectric Strength 7.90 kV/mm
201 kV/in
Step by step; ASTM D149
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade
Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. ..
Dielectric Strength 7.90 kV/mm
201 kV/in
Short Time; ASTM D149
Plenco 4309 Phenolic, Nodular, Injection Molded
PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430..
Dielectric Strength 7.90 kV/mm
201 kV/in
Short Time; ASTM D149
Plenco 7476 Phenolic, Granular, Transfer Molded
PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. ..
Dielectric Strength 7.90 kV/mm
201 kV/in
60 Hz, wet, SS; ASTM D149
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac
FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America...