Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 55.1 kV/mm | >= 1400 kV/in | Short Term; 10 mil film; ASTM D149 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil HDPE HPA 020 Wire & Cable High Density Polyethylene Resin Product Description: HPA 020 is a HDPE grade for Medium/High Voltage power cable jacketing. The grade should be used in blends with LLDPE to improve ESCR. Sufficient Carbon Black or UV stabilizer sh.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin (European Grade) Product Description: LD 100BW is a LDPE containing low antioxidants suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house com.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | 500 V/sec; ASTM D149 |
ExxonMobil LLDPE LL 1002YB Wire & Cable Linear Low Density Polyethylene Resin Product Description: LL 1002YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
ExxonMobil LLDPE LL 4004EL Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 4004EL is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. Sufficient Cu-inhibitor shoul.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | IPC TM-650 2.5.6.2 |
Arlon 35N Fast Cure Polyimide Laminate and Prepreg High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | IPC TM-650 2.5.6.2 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Dielectric Strength | 55.1 kV/mm @Thickness 0.279 mm |
1400 kV/in @Thickness 0.0110 in |
ASTM D149 |
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M |
|||
Dielectric Strength | 55.1 kV/mm | 1400 kV/in | ASTM D149 |
Arlon 32980R015 0.015" (0.381 mm) Uncured Silicon Rubber on Polyester Film Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmProduct Use: Flexible heater substrateAppearance: Red colored, high viscosity gum on polymer liners.. |