Polymer Property : Dielectric Strength = 5.59 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 5.59 kV/mm

@Temperature 121 °C,
Time 10800 sec
142 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
Garlock 706 Compressed Inorganic Fiber Gasketing, Nitrile Binder
Inorganic fibers with a nitrile binder.Inorganic, asbestos-free fibers offer superior performance in saturated and superheated steamThermally stable fibers retain effective seal even during thermal ..
Dielectric Strength 5.59 kV/mm
142 kV/in
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Dielectric Strength 5.59 kV/mm
142 kV/in
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.