Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | ASTM D149 |
LyondellBasell Hifaxâ„¢ AA36H Polypropylene Homopolymer Description: Hifaxâ„¢ AA36H conventional melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabi.. |
|||
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | ASTM D149 |
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil.. |
|||
Dielectric Strength | 42.9 kV/mm @Temperature 23.0 °C |
1090 kV/in @Temperature 73.4 °F |
in oil, short time. 0.25mm; ASTM D149-97a Method A |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | ASTM D149 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |
|||
Dielectric Strength | 42.9 kV/mm | 1090 kV/in | |
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride Hot-pressed boron nitride – aluminum nitride composite that demonstrates high thermal conductivity, dielectric strength, and abrasion resistance. Readily machined and available in rods from 1/4” t.. |