Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Plastcom SLOVAMID 66 GF 15 T 25 PA66, 15% glass fibre, 25% talc FeaturesChemically reinforced with 15% glass fibre and talc, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical in.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Kazanorgsintez 102-16 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Kazanorgsintez 102-17 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Dielectric Strength | >= 40.0 kV/mm | >= 1020 kV/in | Sample of 1 mm thickness, Alternating current |
Kazanorgsintez 108-276 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Dielectric Strength | >= 40.0 kV/mm @Frequency 50.0 Hz |
>= 1020 kV/in @Frequency 50.0 Hz |
For cable masterbatches, at alternating voltage frequency |
Kazanorgsintez P2KP Polyethylene Pigment Masterbatches Production Method: P2KP polyethylene pigment masterbatches are produced on the basis of low density polyethylene with high content of masterbatches. Application: P2KP polyethylene pigment masterbatc.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® B 40 E 000000 Nylon 6 PA 6 extrusion grade, standard grade of high viscosity with processing aid/lubricant, not nucleated. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
Lanxess Durethan® BKV 30 000000 Nylon 6, 30% Glass Fiber 30% Glass fiber reinforced; injection molding grade |
|||
Dielectric Strength | >= 40.0 kV/mm | >= 1020 kV/in | Sample of 1 mm thickness, Alternating current |
Kazanorgsintez 108-278 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | conditioned |
Ineos ABS Triax® KU2-3154 ABS + Nylon 6 Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,Property data per ISO test methods. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243 |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Dielectric Strength | >= 40.0 kV/mm @Frequency 50.0 Hz |
>= 1020 kV/in @Frequency 50.0 Hz |
IEC 60243 |
Borealis Superclean™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable Superclean™ LE4201EHV is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Superclean™ LE4201EHV is intended for insulation of XLPE extr.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | ASTM D877 |
ExxonMobil Univolt N 61B Univolt N 61B is a transformer oil that provides cooling, insulating, arc quenching, and cleaning properties while meeting the requirements of an ASTM D 3487 Type II fluid. Univolt N 61B is a full.. |
|||
Dielectric Strength | 40.0 - 200 kV/mm | 1020 - 5080 kV/in | |
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-15/2 PA6-GF15 Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | ASTM D149 |
Braskem GD5150K HDPE High Density Extrusion Polyethylene GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® N2320 006 POM Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform W 2320 003 UNC Q600 POM Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains .. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | IEC 60243-1 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | |
Kazanorgsintez 153-16 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LBV-50H FWA black 9225 PA12-GF50 Product Description: Grilamid LBV-50H FWA black 9225 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LBV-50H FWA nat PA12-GF50 Product Description: Grilamid LBV-50H FWA natural is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |