Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 21.3 kV/mm | 540 kV/in | Short Term; ASTM D149 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Dielectric Strength | 21.3 kV/mm | 540 kV/in | Method A (Short-time); ASTM D149 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Dielectric Strength | 21.3 kV/mm | 540 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Dielectric Strength | 21.3 kV/mm | 541 kV/in | NF EN 60243.1 |
Isoflon Tisoflon® 10 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Dielectric Strength | 21.3 kV/mm @Thickness 0.635 mm |
540 kV/in @Thickness 0.0250 in |
60 cycles AC avg. RMS; ASTM-D149 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
Dielectric Strength | 21.3 kV/mm | 540 kV/in | ASTM D149 |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Dielectric Strength | 21.3 kV/mm | 541 kV/in | Step by step; ASTM D149 |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |